OK Autrod 18.22


Continuous solid wire suitable for welding of aluminium alloys with more than 3 % Mg, e.g. AlMg4.5Mn, AlMg5Mn and AlMg5Cr, where high tensile strength is required. Can also be used for materials of type AlMgSiCu and AlSi1MgMn and weldable AlZnMg-alloys, like AlZn4.5Mg1. The welding wire has small additions of Zr which increases the fine grained structure of weld deposit and makes it less sensitive to hot cracking during welding.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
25 % 330 MPa 160 MPa

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
26 J 20 °C

Typical Weld Metal Analysis %

MnCuTiSiZrMgAl
0.8 %0.03 %0.03 %0.06 %0.1 %5.8 %92.93 %

Classifications: Wire Electrode

Alloy Type: AlMgMn