ESAB

OK Band 347


OK Band 347 is a stainless welding strip designed for surfacing using the submerged arc welding process. Together with OK Flux 10.05, it produces a 347 type of weld deposit.

Where To Buy


Specifications


Typical Weld Metal Analysis %

MnCNbSiFerrite FNNiNCr
1.8 %0.02 %0.5 %0.37 %11 %10.0 %0.06 %19.5 %

Approvals: NAKS/HAKC, 30x0.5mm, NAKS/HAKC, 60x0.5mm, VdTÜV, 12102
Classifications: AWS A5.9, EQ347, EN ISO 14343-A, B 19 9 Nb

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: IMPERIAL_Austenitic CrNiNb