OK Autrod 13.20 SC


OK Autrod 13.20SC is a Cr-, Mo-alloyed, copper-coated wire for Submerged Arc Welding. Very low level of impurities. X-factor (Bruscato-) max. 11. With OK Flux 10.63 for highest toughness requirements also after Step-Cooling; very clean weld metal with X-factor max. 15. Mainly for creep resistant steels (2,25% Cr, 1% Mo).

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoSCSiCr
0.01 %0.63 %1.00 %0.004 %0.10 %0.16 %2.30 %

Approvals: CE; EN 13479; NAKS/HAKC; 3.0-4.0 mm; CZ; VdTÜV; 12104
Classifications: SFA/AWS A5.23; EB3R