OK Band 309LNb


OK Band 309LNb is a stainless welding strip designed for the submerged arc or electroslag welding process. Together with OK Flux 10.05 it produces a 309LNb type of weld deposit using SAW. In combination with OK Flux 10.14 it manufactures a 347 type of weld deposit using single layer electroslag strip cladding.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnCNbSiFerrite FNNiNCr
1.98 %0.01 %0.7 %0.23 %23 %12.5 %0.03 %23.83 %

Approvals: VdTÜV, 12102
Classifications: EN ISO 14343-A, B 23 12 L Nb

Approvals are based on factory location. Please contact ESAB for more information.