OK Band 309L


OK Band 309L is a stainless welding strip designed for surfacing using the submerged arc strip cladding process. Commonly used as a buffer layer. Often used with OK Flux 10.05.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnCSiFerrite FNNiNCr
1.71 %0.01 %0.36 %15 %13.3 %0.05 %23.72 %

Approvals: NAKS/HAKC; 30x0.5mm; NAKS/HAKC; 60x0.5mm; VdTÜV; 12102
Classifications: EN ISO 14343-A; B 23 12 L; SFA/AWS A5.9; EQ309L

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic 24Cr - 13Ni