Previous Next

ESAB

OK Autrod 19.49


A continuous, solid, Cu-Ni wire for welding similar alloys like 90Cu10Ni, 80Cu20Ni and 70Cu30Ni alloys. The addition of nickel strengthens the weld metal and improves the corrosion resistance, particularly in the case of salt water. The alloy is used for the overlay welding of steels and is widely used for welding Cu-Ni components for desalination plants.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 51 ksi 26 ksi

Typical Weld Metal Analysis %

MnCuCSiNiFe
0.7 %Bal %0.02 %0.05 %31 %0.5 %

Classifications: SFA/AWS A5.7, ERCuNi, Wire Electrode, EN 14640, S Cu 7158 (CuNi30), Wire Electrode