OK Autrod 19.41


A continuous solid aluminium bronze electrode alloyed with Ni. OK Autrod 19.41 is used for overlay welding of steel and for welding of cast or wrought nickel-aluminium bronze materials. The alloy has very good resistance to seawater.

Where To Buy


Specifications


Typical Weld Metal Analysis %

MnCuZnSiNiAlFe
2 %85.00 %0.04 %0.05 %2 %8.0 %2.5 %

Classifications: EN ISO 24373, CuAl8Ni2Fe2Mn2, Wire Electrode

Alloy Type: Alloyed copper (Cu + 8 % Al + 2 % Ni)