Previous Next

ESAB

OK Autrod 19.30


A continuous, solid, copper wire for the GMAW joining of copper-zinc alloys and low-alloyed copper and for the GMAW brazing of zinc-coated steel sheets. OK Autrod 19.30 is alloyed with silicon and manganese and has good flow properties and wear resistance. The alloy is widely used in the joining of zinc-coated steel sheets in car body production, as well as for overlay welding on low- and non-alloyed steels and cast iron. Pulsed GMAW is recommended. OK Autrod 19.30 is normally welded with pure Ar as the shielding gas; however, for GMAW brazing, the addition of 1% O2 improves the brazing properties.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
40 % 51 ksi 19 ksi

Typical Weld Metal Analysis %

MnCuZnSiSnFe
0.9 %96 %0.05 %3 %0.01 %0.05 %

Approvals: VdTÜV, 09147
Classifications: SFA/AWS A5.7, ERCuSi-A, Wire Electrode, EN ISO 24373, CuSi3Mn1, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Alloyed copper (Cu + 3 % Si )