Previous Next

ESAB

OK 67.43

OK 67.43

OK 67.43 is an austentitic, stainless steel, AC/DC electrode, which deposits a weld metal with a small amount of uniformly distributed ferrite. The tough weld metal has excellent crack resistance, even when welding steels with very poor weldability. Suitable for welding 13Mn steels and steels of this kind to other steels.

Where To Buy


Specifications


Typical Tensile Properties

ISO As welded
Elongation Tensile Strength Yield Strength
35 % 91 ksi 64 ksi

Typical Charpy V-Notch Properties

ISO As welded
Impact Value Testing Temperature
59 ft-lb 68 °F
38 ft-lb -76 °F

Typical Weld Metal Analysis %

MnCSiFerrite FNNiNCr
5.4 %0.08 %0.8 %2 %9.1 %0.08 %18.4 %

Approvals: CE, EN 13479, DB, 30.039.07, VdTÜV, 06797
Classifications: EN 14700, E Fe10, EN ISO 3581-A, E 18 8 Mn R 1 2, SFA/AWS A5.4, (E307-16), Werkstoffnummer, 1.4370

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic. CrNiMn
Coating Type: Rutile Basic
Ferrite Content: FN <5
Welding Current: AC, DC+