ESAB

OK 61.25

OK 61.25

OK 61.25 is a basic coated, stainless-steel electrode of the 308H type. The electrode is designed for high-temperature applications in petrochemical and chemical process plants.

Where To Buy


Specifications


Typical Tensile Properties

AWS PWHT 720°C (1328°F) 1000h
Elongation Tensile Strength Yield Strength
45 % 83 ksi 43.5 ksi
AWS As welded
Elongation Tensile Strength Yield Strength
45 % 87 ksi 62 ksi

Typical Charpy V-Notch Properties

AWS PWHT 720°C (1328°F) 1000h
Impact Value Testing Temperature
74 ft-lb 68 °F
AWS As welded
Impact Value Testing Temperature
70 ft-lb 68 °F
61 ft-lb -0.4 °F

Typical Weld Metal Analysis %

PMnMoCuCSSiNiCr
0.03 %1.50 %0.50 %0.50 %0.07 %0.02 %0.45 %10 %19 %

Approvals: Seproz UNA 272580
Classifications: EN 1600; E 19 9 H B 2 2; SFA/AWS A5.4; E308H-15

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic CrNi
Coating Type: Basic
Ferrite Content: FN 2-5