OK Tigrod 16.95


Bare, corrosion-resistant, chromium-nickel-manganese welding rods for welding austenitic stainless alloys of the 18% Cr, 8% Ni, 7% Mn types. OK Tigrod 16.95 has general corrosion resistance similar to that of the corresponding parent metal. The higher silicon content improves the welding properties such as wetting. When used for joining dissimilar materials, the corrosion resistance is of secondary importance. The alloy is used in a wide range of applications across the industry, such as the joining of austenitic, manganese, work-hardenable steels, as well as armour plate and heat-resistant steels.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
41 % 93 ksi 65 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
96 ft-lb 68 °F
41 ft-lb -76 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiNiCr
7.0 %0.20 %0.10 %0.08 %0.9 %8.1 %18.7 %

Approvals: CE; EN 13479; DB; 43.039.12; VdTÜV; 05421
Classifications: EN ISO 14343-A; W 18 8 Mn; Wire Electrode; SFA/AWS A5.9; ER307 mod; Wire Electrode; Werkstoffnummer; ~1.4370; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (18 % Cr - 8 % Ni - 7 % Mn)