OK Band 430


OK Band 430 is a 17Cr welding strip designed for surfacing using the submerged arc welding and electroslag processes. The strip is used mainly for R+M applications. In combination with OK Flux 10.07 is giving a weld metal with 14Cr-4Ni-1Mo and a hardness of 370-420 HB.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnCSiCr
0.66 %0.04 %0.4 %17.0 %

Classifications: EN ISO 14343-A; B 17