OK Band 316L


OK Band 316L is a stainless welding strip designed for surfacing using the submerged arc welding process. Together with OK Flux 10.05, it produces a 316L type of weld deposit.

Where To Buy


Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCSiFerrite FNNiNCr
1.73 %2.9 %0.01 %0.4 %7 %12.6 %0.05 %18.5 %

Approvals: VdTÜV; 12102
Classifications: AWS A5.9; EQ316L; EN ISO 14343-A; B 19 12 3 L

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic CrNiMo