OK Band 308L


OK Band 308L is a stainless welding strip designed for surfacing using the submerged arc welding process. Together with OK Flux 10.05, it produces a 308L type of weld deposit.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

MnCSiFerrite FNNiNCr
1.8 %0.015 %0.3 %12 %10.5 %0.06 %20.0 %

Approvals: VdTÜV, 12102
Classifications: EN ISO 14343-A, B 19 9 L, SFA/AWS A5.9, EQ308L

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic CrNi