OK Autrod 19.12


A continuous, solid, copper wire for the GMAW joining of oxygen-free, pure copper and low-alloyed copper. OK Autrod 19.12 is alloyed with tin and has good flow properties. OK Autrod 19.12 is normally welded with pure Ar as the shielding gas.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
30 % 32 ksi 11 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCuSiFe
0.2 %Bal %0.2 %0.05 %

Approvals: NAKS/HAKC; 1.2MM
Classifications: SFA/AWS A5.7; ERCu; Wire Electrode; EN ISO 24373; CuSn1; Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Copper (Cu + 0.7 % Sn)
x
×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..