Previous Next

ESAB

OK Autrod 16.95


A continous solid corrosion resisting chromium-nickel-manganese wire for welding of austenitic stainless alloys of 18% Cr, 8% Ni, 7% Mn types. OK Autrod 16.95 has a general corrosion resistance similar to that of the corresponding parent metal. The higher silicon content improves the welding properties, such as wetting. The product is a modified variant of ER307, basically with a higher Mn content to make the weld metal less sensitive to hot cracking. When used for joining dissimilar materials the corrosion resistance is of secondary importance. The alloy is used in a wide range of applications across the industry such as joining of austenitic, manganese, work hardenable steels as well as armourplate and heat resistant steels.

Add to shopping list


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
41 % 93 ksi 65 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
96 ft-lb 68 °F

Typical Weld Metal Analysis %

MnMoCuCSiNiCr
7.0 %0.20 %0.10 %0.08 %0.9 %8.1 %18.7 %

Approvals: CE, EN 13479, DB, 43.039.10, NAKS/HAKC, 1.2MM, VdTÜV, 05420
Classifications: EN ISO 14343-A, G 18 8 Mn, Wire Electrode, SFA/AWS A5.9, ER307 mod, Wire Electrode, Werkstoffnummer, ~1.4370, Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic (18 % Cr - 8 % Ni - 7 % Mn)