OK Autrod 12.51


OK Autrod 12.51 is a copper-coated solid wire with higher levels of deoxidizers (manganese and silicon). The high content of deoxidizers allow welding over heavier amounts of dirt, rust, and mill scale while providing a more fluid puddle and smoother bead profile.

Where To Buy


Specifications


Typical Tensile Properties

80% Ar - 20% CO2 As welded
Elongation Tensile Strength Yield Strength Stress Relieved Temperature Stress Relieved Testing Time
26 % 81.2 ksi 69.6 ksi - -
80% Ar - 20% CO2 Stress relieved
Elongation Tensile Strength Yield Strength Stress Relieved Temperature Stress Relieved Testing Time
28 % 71.8 ksi 55 ksi 1148 °F 15 hr

Typical Charpy V-Notch Properties

80% Ar - 20% CO2 As welded
Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
96 ft-lb 68 °F - -
96 ft-lb -4 °F - -
66 ft-lb -22 °F - -
66 ft-lb -40 °F - -
80% Ar - 20% CO2 Stress relieved
Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
88.5 ft-lb 68 °F 1148 °F 15 hr
66 ft-lb -4 °F 1148 °F 15 hr

Typical Weld Metal Analysis %

PMnCSSi
0.01 %1.11 %0.01 %0.01 %0.72 % 0.01 %0.94 %0.08 %0.01 %0.63 %

Approvals: ABS, 3YSA, BV, SA3YM, CE, EN 13479, DB, 42.039.06, DNV-GL, III YMS, LR, 3YS H15, PRS, 3YS, RS, 3YMS, VdTÜV, 00899, CWB, B-G 49A 3 C1 S6 (B-G 49A 3 C G6), PV,ZG, JIS, YGW12, ZG, NAKS/HAKC, 0.8-2.0 mm, PV, NAKS/HAKC, 1.2-1.6 mm, ZG, RINA, 3YS, PV,ZG
Classifications: EN ISO 14341-A, G 38 3 C1 3Si1, Weld Metal, EN ISO 14341-A, G 42 4 M20 3Si1, Weld Metal, EN ISO 14341-A, G 42 4 M21 3Si1, Weld Metal, EN ISO 14341-A, G 3Si1, Wire Electrode, SFA/AWS A5.18, ER70S-6, Wire Electrode, CAN/CSA-ISO 14341, B-G 49A 3 C1 S6, Wire Electrode, JIS Z 3312, YGW 12(C1), Wire Electrode

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Carbon-manganese steel (Mn/Si-alloyed)