OK Autrod 12.24


OK Autrod 12.24 is a copper-coated, molybdenum-alloyed wire for the submerged arc welding of non-alloyed and low-alloyed steels. It can be combined with OK Flux 10.47, OK Flux 10.61, OK Flux 10.62, OK Flux 10.71, OK Flux 10.72, OK Flux 10.73, OK Flux 10.81 and OK Flux 10.83.

Add to shopping list


Specifications


Typical Weld Metal Analysis %

PMnMoSCSiNiCr
0.013 %1.06 %0.50 %0.014 %0.10 %0.15 %0.02 %0.04 %

Approvals: CE, EN 13479, DB, 52.039.06, VdTÜV, 12103, NAKS/HAKC, 3.0, 4,0, 5.0 mm, CZ, NAKS/HAKC, 3.0, 4.0, 5.0 mm, CZ
Classifications: SFA/AWS A5.23, EA2