Previous Next

ESAB

OK 68.53

OK 68.53

OK 68.53 is a coated electrode for welding austenitic-ferritic steels of Super Duplex types, e.g. SAF 2507 and Zeron 100. OK 68.53 has good welding characteristics in all positions and the slag is easily detachable.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
30 % 123 ksi 101.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
37 ft-lb 68 °F
29.5 ft-lb -40 °F

Typical Weld Metal Analysis %

MoCSiFerrite FNNiNCr
4 %0.03 %0.6 %39 %10.3 %0.25 %25.2 %

Approvals: CE, EN 13479, DNV-GL, Duplex, VdTÜV, 07377
Classifications: EN ISO 3581-A, E 25 9 4 N L R 32, SFA/AWS A5.4, E2594-16, Werkstoffnummer, (1.4410)

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Austenitic-ferritic CrNiMo
Coating Type: Basic Rutile
Ferrite Content: FN 35-50
Welding Current: DC+, AC