OK 68.17

OK 68.17

OK 68.17 is a coated electrode designed for the welding of stainless-steel castings of the 13Cr4NiMo type, for example. OK 68.17 can be welded in all positions apart from vertical down.

Where To Buy


Specifications


Typical Tensile Properties

ISO Stress relieved
Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
17 % 1112 °F 8 hr 126 ksi 94 ksi
- 1112 °F 2 hr - -
AWS Stress relieved
Elongation Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
- 1112 °F 1 hr - -

Typical Charpy V-Notch Properties

ISO Stress relieved
Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
33 ft-lb 1112 °F 8 hr 68 °F
33 ft-lb 1112 °F 8 hr 14 °F
29.5 ft-lb 1112 °F 8 hr -40 °F

Typical Weld Metal Analysis %

MnMoCSiNiCr
0.6 %0.6 %0.02 %0.4 %4.6 %12.0 %

Approvals: Seproz, UNA 272580
Classifications: EN 14700, E Fe7, EN ISO 3581-A, E 13 4 R 3 2, SFA/AWS A5.4, E410NiMo-16, Werkstoffnummer, 1.4351

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Martensitic 13Cr4Ni-Mo type
Coating Type: Rutile Basic
Diffusible Hydrogen: <8.0 ml/100g
Welding Current: DC+, AC