ESAB

OK 67.50

OK 67.50

OK 67.50 is an acid rutile coated type for welding of austenitic-ferritic stainless steels of CrNiMoN 22 5 3 - and CrNiN 23 4-types. The duplex all weld metal offers a high strength level combined with good ductility. The pitting corrosion resistance is good and the all weld metal is not sensitive for stress corrosion cracking.

Where To Buy


Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
25 % 124 ksi 100 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
37 ft-lb 68 °F
30 ft-lb -22 °F

Typical Weld Metal Analysis %

MnMoCSiFerrite FNNiNCr
0.8 %3.2 %0.03 %0.8 %42 %8.8 %0.16 %23.2 %

Approvals: ABS, E2209-17, (2.0-3.2mm), ABS, Stainless*, BV, 2209, CE, EN 13479, CWB, CSA W48: E2209-17, DNV-GL, Duplex, RINA, 2209, Seproz, UNA 272580, VdTÜV, 04368
Classifications: EN ISO 3581-A, E 22 9 3 N L R 3 2, SFA/AWS A5.4, E2209-17, CSA W48, E2209-17, Werkstoffnummer, 1.4462

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: Duplex CrNiMoN
Coating Type: Acid Rutile
Ferrite Content: FN 35-50
Welding Current: DC+, AC