OK 67.13

OK 67.13

OK 67.13 is an austenitic, stainless-steel electrode for welding 25Cr20Ni steels. The weld metal resists scaling up to 1100-1150°C and does not contain any measureable ferrite. OK 67.13 can also be used for welding certain air-hardening steels such as armour plate and for welding stainless to unalloyed steel.

Where To Buy


Specifications


Typical Tensile Properties

AWS As welded
Elongation Tensile Strength Yield Strength
35 % 87 ksi 62 ksi

Typical Charpy V-Notch Properties

AWS As welded
Impact Value Testing Temperature
66 ft-lb 68 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCSiNiCr
1.9 %0.12 %0.6 %21.1 %25.6 %

Classifications: EN ISO 3581-A; E 25 20 R 1 2; SFA/AWS A5.4; E310-16; Werkstoffnummer; 1.4842

Alloy Type: Austenitic CrNi
Coating Type: Basic Rutile
Ferrite Content: FN 0
Welding Current: DC+, AC