ARCALOY 309/309H-16

ARCALOY 309/309H-16

Arcaloy 309/309H-16 is used for welding base metal for all service temperatures designed for Type 309. Carbon content 0.04% minimum. It can be used for carbon and low alloy steels and stainless steel dissimilar joints.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Petrochemical

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 90 ksi 55 ksi

Typical Weld Metal Analysis %

MnMoCuCSiFerriteNiCr
1.80 %0.10 %0.10 %0.06 %0.50 %7 FN %13.50 %24 %

Approvals: ABS, AWS A5.4 E309-16, QPL, MIL-E-22200/2 MIL-309-16
Classifications: ASME II SFA E309-16, ASME IX F No. 5, AWS A5.4, E309-16/E309H-16