ARCALOY 309L-16

ARCALOY 309L-16

Arcaloy 309L-16 is used for welding carbon and low alloy steels to stainless steels. This can be done provided the service temperature does not exceed about 700°F (370°C). Post weld heat treatment should only be performed after due consideration.

Where To Buy


Industries

  • Industrial and General Fabrication

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 37 % 85 ksi 65 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiFerriteNiCr
1.80 %0.30 %0.10 %0.03 %0.45 %9 FN %13.50 %23.50 %

Approvals: CWB CSA W48; E309L-16
Classifications: ASME II SFA A5.4; ASME IX F No. 5; AWS A5.4; E309L-16/E309-16