ARCALOY 309L-15

ARCALOY 309L-15

Arcaloy 309L-15 is used for welding carbon and low alloy steels to stainless steels. This can be done provided the service temperature does not exceed about 700°F (370°). Post weld heat treatment should only be taken with great care. Arcaloy 309L-15 can be used as the first layer of stainless steel on carbon or low alloy steel.

Where To Buy


Industries

  • Industrial and General Fabrication

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 45 % 85 ksi 60 ksi

Typical Weld Metal Analysis %

MnCuMoCSiFerriteNiCr
1.8 %0.1 %0.3 %0.035 %0.5 %9 FN %13.5 %24 %

Approvals: ASME II SFA A5.4, E309L-15/E309-15, ASME IX F No. 5, AWS A5.4, E309L-15/E309-15, QPL MIL-E-22200/2 MIL-309L-15
Classifications: AWS A5.4, E309L-15/E309-15