ARCALOY 308/308H-16

Arcaloy 308/308H-16 electrodes were designed for the welding Types 304H & 304 where temperature in excess of 700°F (371°C) requires additional creep strength. They can equally well be used for the welding of stainless steel Types 301, 302 and 305. In some cases where the creep ductility of 347 weld metal is a concern, Arcaloy 308/308H electrodes can be used. The basic-rutile thin coating of Arcaloy 308/308H-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking. Operates on AC or DC current.

Where To Buy


Industries

  • Food and Beverage
  • Industrial and General Fabrication
  • Petrochemical
  • Power Generation
  • Tank and Vessel Fabrication

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 44 % 89 ksi 66 ksi

Typical Weld Metal Analysis %

MnMoCuCSiFerriteNiCr
1.80 %0.30 %0.10 %0.04 %0.50 %9 FN %10 %20 %

Approvals: ABS; AWS A5.4: E308/308H-16; MIL-E-22200/2; MIL-308-16
Classifications: AWS A5.4; E308-16/E308H-16