OK Band NiCrMo3

OK Band NiCrMo3

OK Band NiCrMo3 is a nickel-based strip for submerged arc or electroslag strip cladding. Together with OK Flux 10.11 for electroslag welding or OK Flux 10.16 for subarc welding, produces a weld overlay with good corrosion resistance and high-temperature properties.

Add to shopping list


Welding Process

  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

MnMoCSiNiNb+TaCrFe
0.3 %9.0 %<0.1 %0.1 %≥58.0 %4.0 %22.0 %≤2.0 %

Approvals: VdTÜV, 12102
Classifications: SFA/AWS A5.14, EQNiCrMo-3, EN ISO 18274, B Ni 6625 (NiCr22Mo9Nb)