ARCALOY 308L-16

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 45 % 90 ksi 66 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnMoCuCSiFerriteNiCr
1.70 %0.10 %0.10 %0.03 %0.50 %6 FN %10 %20 %

Approvals: CWB; CSA W48 E308L-16; QPL-22200/2; MIL-308L-16
Classifications: AWS A5.4; E308-16/E308L-16

Approvals are based on factory location. Please contact ESAB for more information.