ESAB

ARCALOY 308L-16

ARCALOY 308L-16

Arcaloy 308L-16 electrodes were developed for the welding of Type 304L stainless steels but can be used for many other stainless steels including Types 301, 302 & 304. They are used extensively for the welding of chemical plant equipment and may be used successfully for the welding of Types 321 and 347 stainless steels provided the service temperature is less than about 700°F (375°C). The basic-rutile thin coating of Arcaloy 308L-16 gives an excellent combination of welding performance in all positions and a high resistance to cracking. Operates on AC or DC current.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Petrochemical
  • Ship/Barge Building
  • Tank and Vessel Fabrication

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 45 % 90 ksi 66 ksi

Typical Weld Metal Analysis %

MnMoCuCSiFerriteNiCr
1.70 %0.10 %0.10 %0.03 %0.50 %6 FN %10 %20 %

Approvals: CWB; CSA W48 E308L-16; QPL-22200/2; MIL-308L-16
Classifications: AWS A5.4; E308-16/E308L-16

Approvals are based on factory location. Please contact ESAB for more information.