OK Band 317L

OK Band 317L

OK Band 317L is a stainless welding strip designed for surfacing using the Submerged Arc Welding process. Together with OK Band 309L and OK Flux 10.05, produces a type 317L weld deposit.

Add to shopping list


Industries

  • Petrochemical
  • Pressure Vessels

Welding Process

  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

MnMoCSiNiNCr
1.26 %3.6 %0.01 %0.45 %14.0 %0.05 %19.0 %

Classifications: EN ISO 14343-A, B 18 15 3 L, SFA/AWS A5.9, EQ317L

Alloy Type: Austenitic 18Cr- 15Ni - 3Mo - L