ATOM ARC 12018

ATOM ARC 12018

Atom Arc 12018 is recommended for use in fabrication of low-alloy, high tensile steels where welds of 120 ksi (830 MPa) minimum tensile strength are required. Atom Arc 12018 is typically used to weld forging, casting plate and pressure vessels.

Where To Buy


Industries

  • Automotive
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Tensile Strength Yield Strength
As Welded 18 % 56 % 133 ksi 120 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 26 ft-lb -60 °F

Typical Weld Metal Analysis %

PMnMoCSSiNiCr
0.014 %1.75 %0.47 %0.057 %0.01 %0.34 %1.97 %0.85 %

Classifications: ASME SFA 5.5, AWS A5.5, E12018M H4R