ESAB

OK FLUX 282

Classifications

AWS - As Welded AWS/EN Wire
F7AZ-EM13K AWS A5.17: EM13K Spoolarc 29S
F7AZ-EM12K AWS A5.17: EM12K Spoolarc 81

Typical Mechanical Properties

Charpy V-Notch Condition Elongation Tensile Strength Wire Yield Strength
14 ft-lb As Welded 22 % 100 ksi Spoolarc 29S 88 ksi
18 ft-lb As Welded 23 % 95 ksi Spoolarc 81 85 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSi
0.03 %1.24 %0.09 %0.02 %0.80 %

Classifications: ASME SFA 5.17; AWS A5.17; F7AZ-EM12K; AWS A5.17; F7AZ-EM13K