ESABs OK Autrod 13.20SC is a copper-coated low alloy submerged arc wire designed for the welding of creep-resistant steel of the (2.5% Cr) (1% Mo) type. When combined with OK Flux 10.63, OK Autrod 13.20SC produces a metalurgically clean weld which is capable of meeting X-factor of less than 15. This combination fulfills the stringent requirements for toughness after step cooling treatment of the weld metal. OK Autrod 13.20SC can also be combined with OK Flux 10.62 for applications not requiring step cooling treatment.~OK Autrod 13.20SC is used for welding process piping, heat exchangers, and pressure vessel fabrication.~

Add to shopping list


Industries

  • Pressure Vessels
  • Process

Welding Process

  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

PMnMoCSSiCr
0.01 %0.63 %1.00 %0.10 %0.00 %0.16 %2.30 %

Approvals: AWS /ASME SFA5.23, EB3R
Classifications: AWS A5.23, EB3R

Approvals are based on factory location. Please contact ESAB for more information.


x
×

Find the Closest Distributor

x

Find the Closest Distributor

x

x

Loading..