SPOOLARC U515

Designed for use on low alloy steels up to 1.25% Cr - 0.5% Mo. Applications include process piping, heat exchangers and pressure vessel fabrication.

Where To Buy


Industries

  • Process
  • Pressure Vessels

Welding Process

  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSiCr
0.01 %0.70 %0.47 %0.10 %0.01 %0.15 %1.20 %

Classifications: ASME SFA 5.23; AWS A5.23; EB2R