SPOOLARC 71

SPOOLARC 71

Spoolarc 71 is a medium manganese and silicon subarc wire that has been microalloyed with titanium. Used with 429, OK 10.62, and OK 10.71 fluxes Spoolarc 71 will produce weld deposits with a minimum 70,000 psi tensile strength in the as welded condition or after eight-hours of stress relief. When used with OK 10.62 weld deposits meet ASME A No. 1 chemistry requirements. Spoolarc 71 is used for welding pressure vessles and can be used for other applications requiring good mechanical properties after stress relieving.

Where To Buy


Industries

  • Pipe Construction
  • Pressure Vessels

Welding Process

  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

PMnCSTiSi
0.01 %1.22 %0.10 %0.01 %0.07 %0.55 %

Classifications: ASME SFA 5.17, AWS A5.17, EM14K