SPOOLARC 81

SPOOLARC 81

Medium manganese and silicon wire - nominal rust and mill scale tolerance. Developed for general purpose welding on low and medium carbon steels. Applications include structural steels, medium strength pressure vessels, ship, barge and offshore oil rig fabrication. Use with OK Flux 429, 231, 350, 10.71, 10.72, and 10.62.

Where To Buy


Industries

  • Windtower
  • Pressure Vessels
  • Ship and Offshore Yards
  • Offshore Oil
  • Structural Steel Fabrication

Welding Process

  • Welding-SAW - Submerged Arc Welding

Specifications


Typical Weld Metal Analysis %

ELEMENTVALUES
PMnCSSi
0.01 %0.95 %0.09 %0.01 %0.26 %

Approvals: ABS; AWS A5.17: EM12K; CWB; CSA W48
Classifications: ASME SFA 5.17; AWS A5.17; EM12K

Approvals are based on factory location. Please contact ESAB for more information.