ARCALOY MC18CrCb

ARCALOY MC18CrCb

Arcaloy MC18CrCb is an 18% Cr alloy metal cored electrode stabilized with Titanium (Ti) and Niobium (Nb). It is designed for welding Armco 18Cr-Cb HP-10TM stainless steels used in catalytic converters, manifolds, mufflers, and exhaust systems. It is also suited for welding parts with poor fit up. Arcaloy MC18CrCb produces a smooth spray-type metal transfer with very minimal spatter.

Where To Buy


Industries

  • Automotive

Welding Process

  • Welding-MCAW - Metal Core Arc Welding
  • Welding-SAW - Submerged Arc Welding
  • Welding-GMAW (MIG/MAG - Metal Inert Gas / Metal Active Gas)

Specifications


Typical Weld Metal Analysis %

98% Ar - 2% O2
PMnCSNbTiSiCr
0.01 %0.70 %0.02 %0.02 %0.50 %0.25 %0.51 %18.60 %
ELEMENTVALUES
PMnCSNbTiSiCr

Classifications: AWS A5.22; EC439Nb