SUREWELD 10P PLUS

SUREWELD 10P PLUS

Sureweld 10P Plus is a modified version of the standard 10P electrode and can be differentiated by its gray coating. It has also been developed for the pipe welding industry but has a more consistent burn-off and a more forgiving arc burn. This provides a better bead profile and sidewall fusion with lower spatter. Sureweld 10P Plus will maintain the proper keyhole in an open root and will produce X-ray quality joints in the flat, horizontal, overhead, vertical-up, and vertical-down procedures. Sureweld 10P Plus is recommended for welding API grades A25, A, B and X42 pipe and general structural, ship, barge and storage tank fabrication. It may also be used for welding root passes in higher grade pipe in some circumstances.

Where To Buy


Industries

  • Civil Construction
  • Industrial and General Fabrication
  • Pipeline

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 25 % 86.9 ksi 72.9 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 33 ft-lb -20 °F

Typical Weld Metal Analysis %

PMnCSSi
0.01 %0.60 %0.15 %0.01 %0.20 %

Approvals: ABS, AWS A5.1: E6010, CWB, CSA W48
Classifications: ASME SFA 5.1, AWS A5.1, E6010

Approvals are based on factory location. Please contact ESAB for more information.