CORE-BRIGHT 309L

CORE-BRIGHT 309L

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 34 % 91 ksi 64 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
MnCSiFerriteNiCr
1.30 %0.02 %0.60 %13 FN %12.80 %24.00 %

Deposition Data

Spray Transfer
Diameter Current Deposition Rate Efficiency (%) TTW Dist. Voltage Wire Feed Speed
3/32 in.
2.4 mm
350 A 13.9 lb/h
6.3 kg/h
88 % 1 in.
25.4 mm
29 V 184 in./min
467 cm/min
3/32 in.
2.4 mm
350 A 17.1 lb/h
7.8 kg/h
87 % 1-1/2 in.
38 mm
29 V 227 in./min
577 cm/min
3/32 in.
2.4 mm
400 A 16.2 lb/h
7.3 kg/h
85 % 1 in.
25.4 mm
30 V 221 in./min
561 cm/min
3/32 in.
2.4 mm
400 A 22.7 lb/h
10.3 kg/h
87 % 1-1/2 in.
38 mm
30 V 302 in./min
767 cm/min
3/32 in.
2.4 mm
450 A 20.6 lb/h
9.3 kg/h
85 % 1 in.
25.4 mm
30 V 273 in./min
693 cm/min
3/32 in.
2.4 mm
450 A 25.9 lb/h
11.7 kg/h
87 % 1-1/2 in.
38 mm
30 V 343 in./min
871 cm/min
.045 in.
1.2 mm
110 A 5.8 lb/h
2.6 kg/h
86 % 3/4 in.
19 mm
26 V 300 in./min
762 cm/min
.045 in.
1.2 mm
150 A 8.1 lb/h
3.67 kg/h
86 % 3/4 in.
19 mm
27 V 400 in./min
1016 cm/min
.045 in.
1.2 mm
180 A 9.8 lb/h
4.45 kg/h
87 % 3/4 in.
19 mm
27 V 500 in./min
1270 cm/min
1/16 in.
1.6 mm
150 A 6.8 lb/h
3.08 kg/h
87 % 3/4 in.
19 mm
27 V 200 in./min
508 cm/min
1/16 in.
1.6 mm
210 A 10.3 lb/h
4.67 kg/h
87 % 3/4 in.
19 mm
28 V 300 in./min
762 cm/min
1/16 in.
1.6 mm
270 A 13.5 lb/h
6.12 kg/h
85 % 3/4 in.
19 mm
29 V 400 in./min
1016 cm/min
5/64 in.
2.0 mm
210 A 7.1 lb/h
3.2 kg/h
86 % 3/4 in.
19 mm
24 V 137 in./min
348 cm/min
5/64 in.
2.0 mm
250 A 9.5 lb/h
4.3 kg/h
87 % 3/4 in.
19 mm
26 V 181 in./min
460 cm/min
5/64 in.
2.0 mm
300 A 12.0 lb/h
5.4 kg/h
85 % 3/4 in.
19 mm
27 V 236 in./min
599 cm/min
3/32 in.
2.4 mm
250 A 8.4 lb/h
3.8 kg/h
85 % 1 in.
25.4 mm
26 V 112 in./min
284 cm/min
3/32 in.
2.4 mm
250 A 10.0 lb/h
4.5 kg/h
89 % 1-1/2 in.
38 mm
26 V 133 in./min
338 cm/min
3/32 in.
2.4 mm
300 A 10.2 lb/h
4.6 kg/h
85 % 1 in.
25.4 mm
28 V 136 in./min
345 cm/min
3/32 in.
2.4 mm
300 A 13.5 lb/h
6.1 kg/h
89 % 1-1/2 in.
38 mm
28 V 178 in./min
402 cm/min

Approvals: ASME SFA 5.22; AWS A5.22; E309LTO-3; CERTIFIED BY C.W.B.- AWS A5.22
Classifications: AWS A5.22; E309LTO-3