CORE-BRIGHT 309L

Designed primarily for overlay applications on carbon steel. May also be used for welding 309 stainless and joining dissimilar metals.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 34 % 91 ksi 64 ksi

Typical Weld Metal Analysis %

MnCSiFerriteNiCr
1.30 %0.02 %0.60 %13 FN %12.80 %24.00 %

Approvals: ASME SFA 5.22, AWS A5.22, E309LTO-3, CERTIFIED BY C.W.B.- AWS A5.22
Classifications: AWS A5.22, E309LTO-3