CORE-BRIGHT 308L

CORE-BRIGHT 308L

Welds types 301, 302, 304, 304L, 321, and 347 stainless steels and austenitic steels. Used extensively for welding chemical plant equipment.

Where To Buy


Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 40 % 90 ksi 62 ksi

Typical Weld Metal Analysis %

MnCSiFerriteNiCr
1.50 %0.03 %0.60 %9 FN %9.90 %19.90 %

Approvals: ASME SFA 5.22, AWS A5.22, E308LTO-3, CERTIFIED BY C.W.B.- AWS A5.22
Classifications: AWS A5.22, E308LT0-3