SHIELD-BRIGHT 2594

SHIELD-BRIGHT 2594

Shield-Bright 2594 is designed for the welding of 25Cr-9Ni-3Mo-0.2N super duplex stainless steel (UNS S32750, S32760). It has excellent slag removal and bead shape with all position welding for use with Ar/CO2 gas mixtures (M21).

Where To Buy


Industries

  • Chemical Industry
  • Offshore Oil
  • Petrochemical
  • Process
  • Pipeline
  • Pulp and Paper

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

As welded
Elongation Tensile Strength Yield Strength
27 % 125 ksi 101.5 ksi

Typical Charpy V-Notch Properties

As welded
Impact Value Testing Temperature
35 ft-lb -20 °F
32 ft-lb -51 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCuCSSiWNiNCr
0.02 %0.95 %3.59 %0.14 %0.03 %0.01 %0.62 %0.02 %9.68 %0.23 %25.34 %

Classifications: SFA/AWS A5.22; E2594T1-4; EN ISO 17633-A; T 25 9 4 N L P M21 2

Alloy Type: Ni, Cr, Mo, N
Welding Current: DC+