ESAB

ATOM ARC 9018

Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 27 % 72 % 1100 °F 24 hr 92 ksi 68 ksi
As Welded 28 % 69 % - - 95 ksi 84 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
As Welded 60 ft-lb -60 °F - -
Stress Relieved 66 ft-lb -60 °F 1100 °F 24 hr

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnMoCSSiNi
0.012 %1.00 %0.29 %0.043 %0.01 %0.26 %1.60 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%) Optimal Amps
3/16 in.
4.8 mm
200-300 A 4.9 lb/h
2.2 kg/h
76.4 % 200 A
3/16 in.
4.8 mm
200-300 A 5.4 lb/h
2.4 kg/h
74.6 % 250 A
3/32 in.
2.4 mm
70-100 A 1.7 lb/h
0.8 kg/h
66.3 % 90 A
1/8 in.
3.2 mm
90-160 A 2.6 lb/h
1.2 kg/h
71.6 % 120 A
1/8 in.
3.2 mm
90-160 A 2.7 lb/h
1.2 kg/h
70.9 % 140 A
5/32 in.
4.0 mm
130-220 A 3.1 lb/h
1.1 kg/h
75 % 140 A
5/32 in.
4.0 mm
130-220 A 3.8 lb/h
1.7 kg/h
73.5 % 170 A

Approvals: ABS; 3Y; LR; 3Ym(H15); QPL-22200/1; MIL-9018-M
Classifications: ASME SFA 5.5; AWS A5.5; E9018M H4R

Approvals are based on factory location. Please contact ESAB for more information.