ATOM ARC 9018

ATOM ARC 9018

Atom Arc 9018 electrodes are used for attachment welds on T-1, HY-80 and HY-90 steels and other high tensile, quenched and tempered steels.

Where To Buy


Industries

  • Bridge Construction
  • Civil Construction
  • Industrial and General Fabrication
  • Mobile Equipment
  • Railcars
  • Ship/Barge Building

Welding Process

  • Welding-SMAW/MMA (Stick)

Specifications


Typical Tensile Properties

Condition Elongation Reduction in Area Stress Relieved Temperature Stress Relieved Testing Time Tensile Strength Yield Strength
Stress Relieved 27 % 72 % 1100 °F 24 hr 92 ksi 68 ksi
As Welded 28 % 69 % - - 95 ksi 84 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature Stress Relieved Testing Temp Stress Relieved Testing Time
As Welded 60 ft-lb -60 °F - -
Stress Relieved 66 ft-lb -60 °F 1100 °F 24 hr

Typical Weld Metal Analysis %

PMnMoCSSiNi
0.012 %1.00 %0.29 %0.043 %0.01 %0.26 %1.60 %

Approvals: ABS; 3Y; LR; 3Ym(H15); QPL-22200/1; MIL-9018-M
Classifications: ASME SFA 5.5; AWS A5.5; E9018M H4R