SHIELD-BRIGHT 309LMO

SHIELD-BRIGHT 309LMO

Shield-Bright 309LMo was designed for welding type 316 clad steels on the first pass in cladding steels or for welding dissimilar metals such as molybdenum-containing austenitic stainless steels to carbon steels. It is used in paper mills and in power plants to give greater corrosion resistance. This wire performs best when used out-of-position shielded with either Argon/C02 or 100% C02.

Where To Buy


Industries

  • Industrial and General Fabrication
  • Process
  • Pulp and Paper

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

C1 Shielding Gas As welded
Elongation Tensile Strength Yield Strength
30 % 90 ksi 70 ksi

Typical Charpy V-Notch Properties

C1 Shielding Gas As welded
Impact Value Testing Temperature
50 J -29 °C
20 J -196 °C

Typical Weld Metal Analysis %

M21 Shielding Gas
PMnMoCSSiNiCr
0.024 %1.2 %2.60 %0.030 %0.008 %0.75 %13.0 %23.5 %
C1 Shielding Gas
PMnMoCSSiNiCr
0.024 %1.0 %2.60 %0.029 %0.008 %0.70 %12.7 %22.90 %

Approvals: DNV-GL, VL 309MoL, KR, RW 309MoLG(C)
Classifications: SFA/AWS A5.22, E309LMoT1-1, Weld Metal, SFA/AWS A5.22, E309LMoT1-4, Weld Metal, JIS Z 3323, TS309LMo-FB1, Weld Metal, KS D 3612, YF309MoLC, Weld Metal, EN ISO 17633-A, T 23 12 2 L P C1 2, Weld Metal, EN ISO 17633-A, T 23 12 2 L P M21 2, Weld Metal

Approvals are based on factory location. Please contact ESAB for more information.


Alloy Type: C Cr Ni Mo
Welding Current: DC+