This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

CORESHIELD 6

CORESHIELD 6

Coreshield 6 is a high productivity, high deposition gasless flux cored wire. This self-shielded wire is ideal for single or multiple pass weld applications in addition to providing high deposition rates, low spatter, and good penetration. Because of its stiffer weld puddle, Coreshield 6 offers exceptional multi-pass weld stacking characteristics, produces excellent bead appearance and X-ray quality weld deposits. Coreshield 6 is run DCEP (electrode positive).

Where To Buy


Industries

  • Ship/Barge Building
  • Bridge Construction
  • Civil Construction

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 26 % 85 ksi 67 ksi

Typical Charpy V-Notch Properties

Condition Impact Value Testing Temperature
As Welded 31 ft-lb -20 °F

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSiNiAl
0.013 %1.26 %0.005 %0.08 %0.13 %0.40 %0.60 %

Approvals: Seismic Certified "D"
Classifications: 5/64 in. (2.0 mm) - AWS A5.36; E70T6-A2-CS3-D H8; 5/64 in. (2.0 mm) - AWS A5.20; E70T-6-D H8; ASME SFA 5.36; ASME SFA 5.20; 3/32 in. (2.4 mm) - AWS A5.36; E70T6-A2-CS3; 3/32 in. (2.4 mm) - AWS A5.20; E70T-6

Approvals are based on factory location. Please contact ESAB for more information.