CORESHIELD 11

Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 22 % 90 ksi 63 ksi

Typical Weld Metal Analysis %

PMnCSSiAl
0.01 %0.60 %0.22 %0.003 %0.21 %1.10 %

Deposition Data

Diameter Current Deposition Rate Efficiency (%) TTW Dist. Voltage Wire Feed Speed
.035 in.
0.9 mm
200 A 4.5 lb/h
2.0 kg/h
81 % 3/8 in.
9.5 mm
17 V 392 in./min
995 cm/min
1/16 in.
1.6 mm
160 A 2.1 lb/h
1.0 kg/h
78 % 5/8 in.
16 mm
17 V 56 in./min
142 cm/min
.035 in.
0.9 mm
80 A 0.9 lb/h
0.4 kg/h
75 % 3/8 in.
9.5 mm
15 V 81 in./min
206 cm/min
1/16 in.
1.6 mm
200 A 2.9 lb/h
1.3 kg/h
80 % 5/8 in.
16 mm
18 V 76 in./min
193 cm/min
1/16 in.
1.6 mm
275 A 5.2 lb/h
2.4 kg/h
81 % 5/8 in.
16 mm
19 V 132 in./min
335 cm/min
5/64 in.
2.0 mm
185 A 2.4 lb/h
1.1 kg/h
77 % 1 in.
25 mm
19 V 50 in./min
127 cm/min
5/64 in.
2.0 mm
250 A 4.5 lb/h
2.0 kg/h
79 % 1 in.
25 mm
20 V 91 in./min
231 cm/min
5/64 in.
2.0 mm
300 A 6.6 lb/h
3.0 kg/h
81 % 1 in.
25 mm
21 V 135 in./min
343 cm/min
.045 in.
1.2 mm
150 A 2.1 lb/h
1.0 kg/h
79 % 1/2 in.
12.5 mm
17 V 118 in./min
300 cm/min
.045 in.
1.2 mm
225 A 2.6 lb/h
1.2 kg/h
82 % 1/2 in.
12.5 mm
18 V 140 in./min
356 cm/min
.045 in.
1.2 mm
95 A 0.9 lb/h
0.4 kg/h
74 % 1/2 in.
12.5 mm
15 V 54 in./min
137 cm/min
.035 in.
0.9 mm
120 A 1.7 lb/h
0.8 kg/h
77 % 3/8 in.
9.5 mm
17 V 155 in./min
394 cm/min

Approvals: CWB, CSA W48 E491T-11-H16
Classifications: ASME SFA 5.36, ASME SFA 5.20, AWS A5.36, E71T11-Z-CS3, AWS A5.20, E71T-11