This site uses cookies and other tracking technologies to provide you with our services, enhance the performance and functionality of our services, analyze the use of our products and services, and assist with our advertising and marketing efforts.

Cookie Policy   Privacy Notice

Previous Next

ESAB

CORESHIELD 40

CORESHIELD 40

Coreshield 40 is a self-shielded flux cored wire primarily designed for multiple pass, horizontal and flat position welding of low and medium carbon steels when toughness is not a requirement. The larger sizes achieve very high deposit rates for very low joining costs. The low penetration, convex fillet bead shape and ability for the slag to desulfurize the deposit make it an ideal choice when crack resistance is a primary consideration. The flat position deposits are smooth and uniform with good wetting into the side walls. The core ingredients are carefully balanced to stabilize the droplet transfer, enhance the ability to handle mill scale and easily detach the slag for quick cleaning. Coreshield 40 is designed to operate on DCEP (electrode positive) with longer electrical stickout. The longer extension increases the deposit potential by preheating the wire.

Where To Buy


Industries

  • Railcars
  • Industrial and General Fabrication
  • Civil Construction

Welding Process

  • Welding-FCAW - Flux Core Arc Welding

Specifications


Typical Tensile Properties

Condition Elongation Tensile Strength Yield Strength
As Welded 29 % 86 ksi 62 ksi

Typical Weld Metal Analysis %

ELEMENTVALUES
PMnSCSiAl
0.012 %0.30 %0.007 %0.20 %0.30 %1.30 %

Classifications: ASME SFA 5.36; AWS A5.36; E70T4-Z-CS3; ASME SFA 5.20; AWS A5.20; E70T-4