COREWELD 110

COREWELD 110

Coreweld 110 is a metal cored electrode designed for single and multipass welding of high strength low alloy steels, such as T-1, HY-80, and HY-100. The arc is smooth with virtually no spatter. Coreweld 110 is recommended for welding quenched and tempered high strength steels. Because of the metallic core, the wire offers both the high deposition rates of a flux cored electrode and the high efficiencies of a solid wire.

Where To Buy


Industries

  • Bridge Construction
  • Ship/Barge Building

Welding Process

  • Welding-MCAW - Metal Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Tensile Strength Yield Strength
As Welded 18 % 112 ksi 96 ksi

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Testing Temperature
As Welded 35 ft-lb 0 °F
As Welded 30 ft-lb -60 °F

Typical Weld Metal Analysis %

PMnMoCSSiNi
0.01 %1.6 %0.5 %0.07 %0.02 %0.35 %2.3 %

Classifications: AWS A5.36, E110T15-M21A6-K3-H4, ASME SFA 5.36, ASME SFA 5.28, AWS A5.28, E110C-K3