COREWELD 80-D2

COREWELD 80-D2

Coreweld 80-D2 is a metal cored wire equivalent to ER80S-D2 solid wire. Coreweld 80-D2 produces higher deposition rates, better wetting action, with an absence of copper coating on the wire. Coreweld 80-D2 was developed for HSLA steels. This product is capable of single or multiple pass welding.

Where To Buy


Industries

  • Automotive
  • Industrial and General Fabrication
  • Mobile Equipment
  • Process

Welding Process

  • Welding-MCAW - Metal Core Arc Welding

Specifications


Typical Tensile Properties

75% Ar - 25% CO2
Condition Elongation Reduction in Area Tensile Strength Yield Strength Stress Relieved Temperature Stress Relieved Testing Time
As Welded 26 % 62 % 90 ksi 77 ksi - -
Stress Relieved 26 % 68 % 90 ksi 77 ksi 1175 °F 8 hr

Typical Charpy V-Notch Properties

75% Ar - 25% CO2
Condition Impact Value Stress Relieved Testing Temp Stress Relieved Testing Time Testing Temperature
Stress Relieved 25 ft-lb 1175 °F 8 hr -20 °F
As Welded 23 ft-lb - - -40 °F
As Welded 34 ft-lb - - -20 °F

Typical Weld Metal Analysis %

75% Ar - 25% CO2
PMnMoCSSi
0.01 %1.6 %0.5 %0.09 %0.01 %0.5 %

Classifications: ASME SFA 5.36, AWS A5.36, E80T15_M21A2-G3, ASME SFA 5.28, AWS A5.28, E80C-G H4